| + | ====== L' | ||
| + | ===== Réglages ===== | ||
| + | source: [[https:// | ||
| + | |||
| + | === Printer Setting === | ||
| + | |||
| + | Make sure your Belt is tensioned enough. Then turn the set screws to approx. half the possible hight and adjust the Y-Endstop, that the nozzle touches the Belt. Then make sure it is leveled (move X to 215 and make the Paper Test). The Paper should be almost not movable (not like with a normal printer), it's important to squeeze the material " | ||
| + | |||
| + | === Temperatures === | ||
| + | |||
| + | I found out, that the belt temperature is like 10°C colder than the bed-heater temp. So you should always add ~10°C to the Bed-Temp of your material (70°C for PLA). That way, you will have very good adhesion and you will see, that the model will stick more to the belt than you would like to :) It happens, that I have to move the Belt to remove my prints sometimes. | ||
| + | |||
| + | The Standard Temperatures (240/75) are overridden by the Material Settings! | ||
| + | |||
| + | |||